EVALUATION OF LB-2 DIFFUSION - COATINGS ON TANTALUM,

reportActive / Technical Report | Accession Number: AD0431623 | Need Help?

Abstract:

Tantalum material 0.045 in. thick can be satisfactorily LB-2 diffusion coated by applying 1020 mils per side of LB-2 base coat slurry and diffusing per MAC P S 13156, Revision C. The 0.006 in. material should be coated employing smaller slurry coating thicknesses than 7 mils per side perhaps 2 or 3 mils. Author