DID YOU KNOW? DTIC has over 3.5 million final reports on DoD funded research, development, test, and evaluation activities available to our registered users. Click
HERE to register or log in.
Accession Number:
AD0852171
Title:
Hydrolytic Stability of Elastomeric Materials.
Descriptive Note:
Phase rept. no. 2,
Corporate Author:
NAVAL AIR DEVELOPMENT CENTER WARMINSTER PA AERO MATERIAS DEPT
Report Date:
1969-03-18
Pagination or Media Count:
25.0
Abstract:
Seven elastomeric materials were exposed in a high temperature-high humidity environment 200F, 95 R.H. for various intervals, through 28 days. Deterioration varied greatly and most of the materials reached a plateau a leveling-off of degradation which occurred approximately at the 7-day interval. Several comparative environments were studied, including a cycling procedure simulating operational conditions. Author
Distribution Statement:
APPROVED FOR PUBLIC RELEASE