Abstract:

Among the basic defects found in large area thin wall castings made by the press casting method are included the following 1 heavy walls, 2 waviness, 3 dynamic pressure cracks, 4 blow holes, and 5 shrinkage cracks. A brief description of these defects is given below also the basic measures for their prevention are shown. Author